Pláta 800h Incoloy

 

Is é JN Alloy an soláthróir pláta is mó de Incoloy 800h le fardal ollmhór de phláta rollaithe te 800h, ASTM B409 Pláta snasta agus pláta rolladh fuar 800h. Tairgimid cornaí DIN 1.1958/1.4876 i méideanna éagsúla ar an bpraghas is fearr. Táimid i gceannas ar an monaróir de chuid Incoloy Alloy 800h Strip & Incoloy 800h.

 

Incoloy 800H is an iron-nickel-chromium alloy having the same basic composition as Incoloy 800, with significantly higher creep rupture strength. Sheets and plates made of Incoloy 800H have a stiff structure, contributing to increased temperature stability. They contain aluminum and titanium, providing corrosion resistance and preventing carburization precipitation in heat-working applications. Sheets and plates made of Incoloy 800H offer excellent erosion, corrosion, and oxidation resistance in media and perform well in applications involving constant high temperatures. The higher strength results from close control of carbon, aluminum and titanium contents in conjunction with a high temp anneal. The 800H modification was to control carbon (0.05 to 0.10%) and grain size to (>ASTM 5) chun airíonna réabtha struis a bharrfheabhsú. Tá modhnuithe breise ag Incoloy 8 0 0h ar na leibhéil tíotáiniam agus alúmanaim chomhcheangailte (0.85 go 1.2%) chun airíonna ardteochta is fearr a chinntiú. Tá an cóimhiotal dé -dheimhnithe agus comhcheanglaíonn sé airíonna an dá fhoirm. Ní dhéanfar pláta Incoloy 800h a chur i bhfeidhm fiú tar éis úsáid fhada an chóimhiotail idir an raon teochta de 1200 - 1600 céim F, ag an gcéim a bhíonn ag go leor gráid cruach dhosmálta.

 

Soláthraíonn cóimhiotail JN an pláta 800h is fearr. Is soláthróirí iad na bileoga agus na plátaí cruach is fearr in Incoloy 800h. Is iad an cóimhiotal cruach dhosmálta Incoloy 800h a mhonaraíonn na bileoga agus na plátaí seo, a bhfuil go leor de na hairíonna is mó aige. Fágann sé seo go bhfuil siad an -úsáideach le haghaidh feidhmchlár láidir tionsclaíoch. Tá neart níos airde agus friotaíocht iontach ag na bileoga agus na plátaí seo. Is éard atá sna plátaí seo ná nicil agus cróimiam. Leis na heilimintí seo a bheith i láthair, éiríonn na plátaí cóimhiotail 800h seo níos frithsheasmhaí do chreimeadh mar gheall ar fhachtóirí difriúla cosúil le creimeadh, taise agus ceimiceáin. Tá na bileoga plátaí 800h incoloy seo an -insínte agus intuargainte i nádúr. Tá neart teanntachta agus neart táirgeachta níos mó acu freisin. Dá bhrí sin, níl aon scoilteadh acu. Tá siad frithsheasmhach freisin don athrú airíonna ag teocht níos airde. Táimid ag soláthar caighdeán níos fearr na mbileog agus na bplátaí do na cliaint go léir atá ar fáil ar fud na cruinne. I measc na ndaoine is stoic, tá muid i measc na n -onnmhaireora agus an onnmhaireora iontaofa ar chaighdeán na mbileog agus na bplátaí.

 

Sonraíocht Pláta 800h Incoloy

 

Sonraíochtaí Sonraíochtaí

ASTM B409 / ASME SB409

Sonraíocht tríthoiseach

Jis, AISI, ASTM, GB, DIN, EN, srl

Leithead

1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, srl

Tiús

4mm -100 mm

Ar fad

2000mm, 2440mm, 3000mm, 5800mm, 6000mm, srl

Bailchríoch

2B, 2D, BA, Uimh.1, Uimh.4, Uimh.8, 8K, Scáthán, Checkered, Placossed, Hairline, Blast Gaineamh, Scuab, Eitseáil, Pláta Rolladh Te (HR), Bileog Fuar Rolladh (CR), Satin (le plaisteach brataithe) srl.

Cré

Bog, crua, leath crua, ráithe crua, earrach crua srl.

Gnáthnós

Cornaí, scragaill, rollaí, leathán plain, bileog shim, bileog bréifneach, pláta, stiall, árasáin, bán (ciorcal), fáinne (flange) srl.

Bailchríoch

Uimh.1, Uimh.4, Uimh.

 

Pláta 800h Incoloy, Bileog & Comhdhéanamh Ceimiceach Coil

 

Grád

C

MN

SI

S

Rise

Fe

Ni

Cc

Bal de

Tí

800H

0.05 – 0.10

1.50 Max

1. 00 max

{0. 015 max

{0. 75 max

39.50 nóiméad

30.00 – 35.00

19.00 – 23.00

0.15 – 0.60

0.15 – 0.60

 

ARTM B409 UNS N08810 Pláta Airíonna Meicniúla

 

Eilimint

Dlús

Leáphointe

Neart teanntachta

Neart Toradh (0. 2%Fritháireamh)

Élagáil

800H

7.94 g/cm3

1385 céim (2525 céim F)

PSI - 75, 000, MPA - 520

PSI - 30, 000, MPA - 205

30 %

 

Ábhar coibhéiseach de phláta 800h Inconel 800h

 

Caighdeánach

Werkstoff nr.

Léimneach

Iiosaean

Bs

Gast

Ar fhaoiseach

Ein

Nó

Incoloy 800h

1.4958 / 1.4876

N08810

NCF 800h

Na 15 (h)

ЭИ670

Z8nc 33-21

X5nicralti 31-20

XH32T

 

Iarratais 800h Alloy Incoloy

 

Coirí múchta foirnéise eitiléine

Próiseáil cheimiceach agus peitriceimiceach

Scoilteadh hidreacarbóin

Super-téitheoir agus ath-théithe i ngléasraí cumhachta

Comhlaí, feistis agus comhpháirteanna eile a nochtar ionsaí creimneach ó 1100-1800 Céim f

Soithí brú

Foirnéisí tionsclaíocha

Malartóirí teasa

Trealamh Cóireáil Teasa

 

Teacht chugainn
Agus tús a chur le do RFQanna anois.